| TYPICAL PROPERTIES OF
TOYOLAC 450Y MH1 |
| Typical Properties |
|
Test Method |
|
Test Conditions |
|
Unit |
|
Typical Value |
| Melt Flow Rate |
|
ISO 1133 |
|
220 oC/10kg |
|
g/10min |
|
4 |
| Charpy Impact, notched |
|
ISO 179 / 1eA |
|
23oC |
|
kJ/m2 |
|
14 |
| Deflection Temperature Under Load |
|
ISO 75 |
|
120oC/hr,
1.8MPa |
|
oC |
|
98 |
| Tensile Yield Stress |
|
ISO 527 |
|
50 mm/min |
|
MPa |
|
46 |
| Tensile Elongation |
|
ISO 527 |
|
50 mm/min |
|
% |
|
>10 |
| Tensile Modulus |
|
ISO 527 |
|
1 mm/min |
|
MPa |
|
2300 |
| Flexural Stress |
|
ISO 178 |
|
2 mm/min |
|
MPa |
|
69 |
| Density |
|
ISO 1183 |
|
|
|
kg/m3 |
|
1070 |